Mineral and metallic abrasives for blasting, surface preparation and waterjet cutting.

Mineral abrasives

Metallic abrasives

Plastic abrasives

Comparison

Technical values side by side

Hardness is given on the Mohs or HRC scale depending on the product type; the two scales cannot be compared directly.

ProductShapeHardnessDensityGrain rangeGrading
White Aluminium OxideAngular and irregularMohs 93.9 – 4.1 g/cm³0.09 – 0.85 mmFEPA
Brown Aluminium OxideAngular and sharpMohs 9~3.9 g/cm³0.045 – 2.8 mmFEPA
Garnet—Mohs 7.5 – 8.03.9 – 4.2 g/cm³0.1 – 0.85 mmMesh
Glass AbrasiveAngular or roundedMohs 5.5 – 6~2.5 g/cm³0.2 – 2 mmmm
Steel ShotRound~20 HRC (new) / ~45 HRC (after use)~7 g/cm³0.0 – 1.7 mmDesignation no.
Steel GritAngular40 – 68 HRC (390 – 740 HV)7.8 g/cm³0.18 – 2.4 mmSAE
Stainless Steel ShotRound————
Stainless Steel GritAngular~59 HRC (710 HV)~7.0 g/cm³0.0 – 2.5 mmDesignation no.
Nickel GritAngular and sharp~55 – 65 HRC~7.5 g/cm³0.18 – 2.4 mmNG
Glass BeadsSphericalMohs 5.5 – 6~2.5 g/cm³0.04 – 0.84 mmmm
Black Silicon CarbideAngular and sharpMohs 9 – 9.5~3.2 g/cm³0.045 – 0.85 mmFEPA
Cylindrical Cut Wire ShotCylindrical~40 – 55 HRC~7.8 g/cm³0.4 – 2 mmWire diameter (mm)
Conditioned Cut Wire ShotRounded~45 – 65 HRC~7.8 g/cm³0.4 – 1.6 mmWire diameter (mm)
Plastic GranulesAngularMohs ~3 – 4~1.5 g/cm³0.25 – 1.7 mmMesh
Quartz SandAngular or roundedMohs 7~2.65 g/cm³0.1 – 2 mmmm
Mixed AluminaAngularMohs ~9~3.9 g/cm³0.09 – 0.85 mmFEPA
Basalt SandAngular – semi-angularMohs ~6 – 6.5~2.8 – 3.0 g/cm³ (rock)0.5 – 3 mmmm