Anadolu Kumlama Quartz Sand is a natural silica-based mineral. Important warning: using quartz sand in dry blasting creates respirable crystalline silica dust, which can cause serious lung diseases such as silicosis, and its use for blasting is restricted in many countries. Check the legislation in force before use; do not use it without suitable dust control and respiratory protection.

Technical specifications

Material
Quartz (SiO₂)
Hardness
Mohs 7
Density
~2.65 g/cm³
Colour
White, cream or yellowish
Occupational safety
Carries a risk of respirable crystalline silica

Typical grain sizes

Grain sizeApplication
0.1 – 0.4 mmFine work
0.4 – 0.8 mmGeneral use
0.8 – 1.2 mmCoarse work
1.2 – 2.0 mmHeavy work

Blasting applications

  • Wet blasting systems
  • Enclosed systems with dust control
  • Cleaning work requiring low hardness
  • Non-blasting industrial applications

Advantages

  • A natural, widely available mineral
  • Different grain ranges
  • Contact our sales team about safer alternatives for blasting

For open-air blasting or work without dust control, we recommend considering garnet, aluminium oxide or metallic abrasives. Values are typical industry figures; contact our sales team for the product data sheet and current grain options.

Which material and grain size suit your job?

Tell us about your surface, your blasting system and the quantity you need, and our sales team will get back to you.