Blasting abrasives supplier
+90 216 706 70 72+90 532 063 81 58info@anadolukumlama.com

Mineral abrasives

Brown Aluminium Oxide

Hard, angular grains and a wide range of grain sizes.

Brown Aluminium Oxide, close-up view

Brown aluminium oxide is one of the most preferred abrasives in industrial blasting. Belonging to the fused alumina group, it is produced by melting bauxite and anthracite at high temperature. Its angular, hard structure gives surfaces an aggressive abrasive action. The fact that it contains no silica makes it a safer alternative in terms of health.

Technical specifications

Chemical composition
Al₂O₃ > 95%, Fe₂O₃ < 0.3%, SiO₂ < 1.2%
Hardness
Mohs 9
Density
~3.9 g/cm³
Colour
Brown
Shape
Angular, sharp grains

Grain sizes and applications

FEPA codeSize range (µm)Application
F 082000 – 2800Heavy industrial cleaning
F 24600 – 850General surface cleaning
F 60212 – 300Medium-level roughening
F 12090 – 125Precision surface treatment
F 22045 – 75Fine detail blasting

Blasting applications

  • Rust and paint removal
  • Matting of metal surfaces
  • Decorative processing of glass and ceramics
  • Surface preparation of automotive parts
  • Production of sandpaper and abrasive stones
  • Surface roughening before coating and welding

Advantages

  • Fast and effective cleaning with high abrasive power
  • Safe use on stainless steels because it contains no iron
  • Compatible with wet and dry blasting systems
  • Reusable, long-lasting and economical
  • Provides occupational safety with low dust generation
  • Environmentally friendly and recyclable

Brown aluminium oxide blasting media is an ideal choice in terms of high performance, low cost and environmental sustainability. Thanks to its wide choice of grain sizes and applications, it can be used with confidence in both heavy industry and precision surface treatment.

Related posts

Which material and grain size suit your job?

Tell us about your surface, your blasting system and the quantity you need, and our sales team will get back to you.