Conditioned Cut Wire Shot

Rounded-edge grains for consistent surface hardening.

Conditioned Cut Wire Shot, close-up view

Anadolu Kumlama Conditioned Cut Wire Shot is a metallic abrasive made by rounding the edges of cut steel wire. Its regular grain structure ensures consistent impact. It is therefore used especially for surface hardening of springs, gears and similar loaded parts.

Technical specifications

Material
Carbon or stainless steel wire
Shape
Rounded edges (conditioned)
Hardness
~45 – 65 HRC
Density
~7.8 g/cm³

Typical wire diameters

Wire diameter (mm)Application
0.4 – 0.6Small precision parts
0.6 – 0.8Small springs and gears
0.8 – 1.2General surface hardening
1.2 – 1.6Large parts

Blasting applications

  • Surface hardening of springs and gears (shot peening)
  • Improving the fatigue strength of loaded parts
  • Precision cleaning
  • Turbine and pressure systems

Advantages

  • Regular grain structure and consistent impact
  • Controlled process, as there are no sharp edges
  • Long service life
  • High-hardness options

Conditioned Cut Wire Shot is a strong option for surface hardening where repeatable results are required. Values are typical industry figures; contact our sales team for the product data sheet and current grain options.