Compare all productsMineral abrasives

White Aluminium Oxide
High purity, iron-free structure, precision surface treatment.
- Hardness
- Mohs 9
- Density
- 3.9 – 4.1 g/cm³

Brown Aluminium Oxide
Hard, angular grains and a wide range of grain sizes.
- Hardness
- Mohs 9
- Density
- ~3.9 g/cm³

Garnet
A natural, almandine-based abrasive, from blasting to waterjet cutting.
- Hardness
- Mohs 7.5 – 8.0
- Density
- 3.9 – 4.2 g/cm³

Glass Abrasive
Made from recycled glass, for industrial and decorative use.
- Hardness
- Mohs 5.5 – 6
- Density
- ~2.5 g/cm³

Glass Beads
Spherical grains, a satin finish and cleaning without dimensional change.
- Hardness
- Mohs 5.5 – 6
- Density
- ~2.5 g/cm³

Black Silicon Carbide
Very high hardness and sharp grains for demanding surfaces.
- Hardness
- Mohs 9 – 9.5
- Density
- ~3.2 g/cm³

Quartz Sand
Natural silica sand; to be used only with suitable protection and systems.
- Hardness
- Mohs 7
- Density
- ~2.65 g/cm³

Mixed Alumina
A mix of aluminium oxide types for general-purpose blasting.
- Hardness
- Mohs ~9
- Density
- ~3.9 g/cm³

Basalt Sand
A volcanic, economical, non-metallic abrasive for general-purpose work.
- Hardness
- Mohs ~6 – 6.5
- Density
- ~2.8 – 3.0 g/cm³ (rock)
Metallic abrasives

Steel Shot
Cleaning and surface hardening through controlled impact.
- Hardness
- ~20 HRC
- Density
- ~7 g/cm³

Steel Grit
Angular structure, aggressive cleaning and a profile for coating.
- Hardness
- 40 – 68 HRC
- Density
- 7.8 g/cm³

Stainless Steel Shot
A round-grained stainless metallic abrasive.
Contact us for technical data

Stainless Steel Grit
Processing delicate metals without creating a corrosion risk.
- Hardness
- ~59 HRC
- Density
- ~7.0 g/cm³
Representative imageNickel Grit
Heavy-duty power for rusty and thickly coated surfaces.
- Hardness
- ~55 – 65 HRC
- Density
- ~7.5 g/cm³

Cylindrical Cut Wire Shot
Cylindrical grains cut from steel wire for long-lasting cleaning.
- Hardness
- ~40 – 55 HRC
- Density
- ~7.8 g/cm³

Conditioned Cut Wire Shot
Rounded-edge grains for consistent surface hardening.
- Hardness
- ~45 – 65 HRC
- Density
- ~7.8 g/cm³
Plastic abrasives
Looking for a blasting service?
As well as abrasives, you can request a quote for blasting services. Describe your surface and job, and we will get back to you.
Applications
Start from your application
Choose an application area to see the products used for that job.
Shipbuilding and marine
Pre-coating preparation
Steel GritSurface roughening and pre-coating preparation
Brown Aluminium OxideSurface roughening before coating and welding
White Aluminium OxideSurface roughening before painting and coating
Steel ShotSurface preparation before welding and coating
Stainless Steel GritSurface preparation before coating, painting and metallising
Mixed AluminaSurface roughening before coating
Basalt SandIndustrial surface preparation
Stainless and non-ferrous metals
Casting and forging
Petrochemicals and pipelines
Concrete and stone
Glass and decorative
Glass AbrasiveDecorative frosting of glass surfaces
GarnetDecorative processing of glass and ceramic surfaces
Brown Aluminium OxideDecorative processing of glass and ceramics
Stainless Steel GritDecorative processing of marble and stone surfaces
Black Silicon CarbideProcessing of glass, stone and ceramic surfaces
Waterjet cutting
Surface hardening
Grain size
Grain ranges covered by our products
From coarse cleaning to fine detail blasting, the range of each product on a single scale.
References
Organisations we work with
- Aselsan
- Makine ve Kimya Endüstrisi Anonim Şirketi
- Akkuyu Nuclear Power Plant
Certificates
Management system certificates
- ISO 9001:2015Quality Management System
- ISO 14001:2015Environmental Management System
- ISO 45001:2018Occupational Health and Safety Management System
- ISO 22301:2019Business Continuity Management System
- ISO 31000:2018Risk Management System
- ISO 10002:2018Customer Satisfaction and Complaints Management System
- ISO 26000:2021Social Responsibility Management System
- Respect for NatureRespect for Nature Certificate
Blog
Latest posts
All posts
Guide
How to Choose a Blasting Abrasive
Surface material, desired result, blasting system and occupational safety: the four key criteria for choosing the right abrasive.
Read more

Guide
The Difference Between Steel Shot and Steel Grit
One is round, the other angular: steel shot and steel grit give different results on the surface. We compare which suits which job.
Read more

Technical Information
What Are Sa 2, Sa 2½ and Sa 3? A Guide to Cleanliness Grades
What do the Sa grades in blasting specifications mean? We explain the cleanliness grades of ISO 8501-1 and how they differ from surface profile.
Read more
Which material and grain size suit your job?
Tell us about your surface, your blasting system and the quantity you need, and our sales team will get back to you.