Anadolu Kumlama Glass Beads are a spherical glass abrasive. Because they work the surface by impact rather than by cutting, they preserve part dimensions while giving a clean, bright or satin appearance. They are preferred for stainless steel, aluminium and precision metal parts.

Technical specifications

Material
Soda-lime glass
Shape
Spherical
Hardness
5.5 – 6 on the Mohs scale
Density
~2.5 g/cm³
Colour
Transparent

Typical grain sizes

Grain sizeApplication
0.04 – 0.07 mmVery fine finish
0.07 – 0.11 mmFine satin finish
0.15 – 0.25 mmGeneral satin finish
0.25 – 0.42 mmGeneral cleaning
0.42 – 0.84 mmStronger cleaning

Blasting applications

  • Satin finish on stainless steel and aluminium parts
  • Cleaning of precision parts
  • Removal of weld seams and heat tint
  • Surface hardening of small parts (glass bead peening)

Advantages

  • No significant change in part dimensions
  • Gives a uniform, decorative finish
  • Causes no iron contamination
  • Reusable under suitable conditions

Glass Beads deliver a clean, controlled result where surface appearance and part dimensions matter. Values are typical industry figures; contact our sales team for the product data sheet and current grain options.