Brown fused alumina FeSi is an alternative whenever you want to make use of the typical alumina properties but the product does not have to be iron-free. The combination of hardness and high weight make this blasting medium powerful.
Technical specifications
- Product code
- FeSi
- Hardness
- 9 mohs
- Grain shape
- angular
- Melting point
- ca. 1.500 °C
- Specific gravity
- ca. 5.5 g/cm³
- Bulk density (depending on grain size)
- ca. 2.2 – 3.0 g/cm³
- Typical Chemical Analysis
- Al₂O₃ 39.00 % · TiO₂ 0.90 % · Fe₂O₃ 0.30 % · SiO₂ 0.30 % · Fe 46.00 % · Si 7.20 % · Ti 3.00 %
- Packaging
- 25 kg bags on 1t pallets; 1 ton loose in a big bag
- Blasting Systems
- Pressure blast machines, Vacuum blast machines
Available sizes
| Average grain size (mm) |
|---|
| 0.12 – 0.25 |
| 0.25 – 0.50 |
| 0.50 – 1.00 |
| 0.50 – 1.50 |
| 1.00 – 1.50 |
| 1.00 – 2.00 |
Blasting applications
- Multi-purpose blasting abrasives
- Wear protection
Other grain sizes can be produced if required.