Blasting abrasives supplier
+90 216 706 70 72+90 532 063 81 58info@anadolukumlama.com

Organic abrasives

Nutshell granules

Soft, organic and renewable abrasive for surface work with low impact on the base material.

Nutshell granules, close-up view

Nutshell granules are an extremely soft, organic reusable blasting agent made from broken, cleaned and sieved walnut shells. Due to their low hardness, the nutshell granules are used mainly for surface applications where loss of substance in the base material is not wanted. Nutshell granules are made from walnut shells, a renewable raw material.

Technical specifications

Hardness
ca. 2.5 – 3.5 mohs
Grain shape
angular
Ignition temperature
ca. 170 °C
Specific gravity
ca. 1.0 – 1.2 g/cm³
Bulk density (depending on grain size)
ca. 0.45 – 0.8 g/cm³
Typical Chemical Analysis
Packaging
25 kg bags on 1t pallets; 1 ton loose in a big bag
Blasting Systems
Pressure blast machines, Vacuum blast machines

Available sizes

DesignationAverage grain size (mm)
2/120.10 – 0.20
6/120.20 – 0.45
4/60.45 – 0.80
3/60.45 – 1.00
16/50.80 – 1.30
15/101.00 – 1.50
12/31.00 – 1.70
12/3E1.30 – 1.70
CAG 16/101.70 – 2.40
8/102.40 – 4.00
1/274.00 – 6.00

Blasting applications

  • Additive for oil binders
  • Dry abrasive

Other grain sizes can be produced if required.