Our stainless steel cut wire with chrome and nickel is not only used for shot peening but also in granite stone processing. This product is valued for its longevity and its corrosion protection properties.
Technical specifications
- Product code
- CrNi
- Hardness
- Depending on grain shape and grain diameter (approx. 400 – 670 HV)
- Grain shape
- cylindrical/rounded
- Melting point
- ca. 1.450 – 1.500 °C
- Specific gravity
- approx. 6.5 – 7.8 g/cm³
- Bulk density (depending on grain size)
- approx. 3.8 – 4.8 g/cm³
- Typical Chemical Analysis
- Cr 11.50 – 20.0 % · Mn max. 7.50 % · Si max. 1.00 % · C max. 0.15 % · P max. 0.06 % · S max. 0.030 % · Ni max. 10.0 % · Fe rest
- Specifications
- DIN 8201-4; SAE AMS 2431/4; SAE J441
- Packaging
- 25 kg sacks on pallet up to 1 t; 1 t loose in a big bag
- Blasting Systems
- Pressure blast systems, Wheel blasting systems
Available sizes
| Diameter (mm) |
|---|
| 0.3 |
| 0.4 |
| 0.5 |
| 0.6 |
| 0.7 |
| 0.8 |
| 0.9 |
| 1.0 |
| 1.2 |
| 1.4 |
| 1.6 |
Blasting applications
- Blast cleaning
- Concrete and natural stone cleaning
- Deburring
- Descaling
- Fettling
- Sand removal
- Surface preparation
Advantages
- Reusable abrasive
Other grain sizes can be produced on request.