Chilled cast iron angular

Very hard, angular grit made from chilled cast iron.

Chilled cast iron angular, close-up view

Chilled cast iron angular is particularly suitable for processing metallic surfaces in pressure blasting machines. Due to its hardness and high carbon content, chilled cast iron repeatedly breaks into sharp-edged particles, which leads to a very high abrasive performance with short blasting times.

Technical specifications

Hardness of the new grain
640 – 900 HV (57 – 67 HRC)
Grain shape
angular
Melting point
ca. 1.535 °C
Specific gravity
ca. 7 g/cm³
Bulk density (depending on grain size)
ca. 3.0 – 4.6 g/cm³
Microstructure
martensitic
Typical Chemical Analysis
C 2.70 – 3.40 % · Si 0.80 – 2.00 % · Mn 0.25 – 1.00 % · P 0.10 – 1.50 % · S 0.06 – 0.25 % · Fe Remainder
Specifications
EN ISO 11124-2; DIN 8201-3; BS 2451
Packaging
25 kg bags on 1t pallets; 1 ton loose in a big bag
Blasting Systems
Pressure blast machines, Wheel blast machines (wear protection recommended)

Available sizes

DesignationAverage grain size (mm)
G 020.1 – 0.2
G 050.1 – 0.3
G 070.2 – 0.4
G 120.3 – 0.6
G 170.4 – 0.8
G 240.6 – 1.0
G 340.8 – 1.2
G 391.0 – 1.4
G 471.2 – 1.7
G 551.4 – 2.0
G 661.7 – 2.4
G 802.0 – 2.8

Blasting applications

  • Paint stripping
  • Preparation for surface coating
  • Rough blasting
  • Rust removal

Other grain sizes can be produced if required.