PA abrasive

Polyamide granules for deburring thermoset, rubber and silicone parts.

PA abrasive, close-up view

Polyamide is used mainly as an abrasive for deburring parts made of thermoset. As polyamide is comparatively soft, its effect on plastic surfaces is low; suitability should be confirmed by a trial.

Technical specifications

Product code
PA
Hardness
2 – 3 mohs
Grain shape
cylindrical/ cubical
Melting point
ca. 215 – 225 °C
Specific gravity
ca. 1.08 – 1.60 g/cm³
Bulk density (depending on grain size)
ca. 0.7 g/cm³
Typical Chemical Analysis
Plastics from Polyamide 6, additives < 1 %
Packaging
25 kg bags on 1t pallets
Blasting Systems
Pressure blast machines, Vacuum blast machines, Wheel blast machines

Available sizes

Size in mm (diameter x length)
0.50 x 0.50
0.75 x 0.75
1.00 x 1.00
1.00 x 1.50
1.50 x 1.00
1.50 x 1.50
2.00 x 2.00
0.50 x 0.50
0.60 x 0.60
0.75 x 0.75
1.00 x 1.00
1.20 x 1.20
1.50 x 1.50

Blasting applications

  • Rubber deburring
  • Silicone deburring
  • Thermoset deburring

Colour: red, nature