Chilled iron shot is a spherical metallic material made from chilled cast iron. Besides blasting, it is used in heavy concrete, pyrotechnics and radiation protection.
Technical specifications
- Hardness of the new grain
- 640 – 900 HV (57 – 67 HRC)
- Grain shape
- spherical
- Melting point
- ca. 1.535 °C
- Specific gravity
- ca. 7 g/cm³
- Bulk density (depending on grain size)
- ca. 3.0 – 4.6 g/cm³
- Microstructure
- martensitic
- Typical Chemical Analysis
- C 2.70 – 3.40 % · Si 0.80 – 2.00 % · Mn 0.25 – 1.00 % · P 0.10 – 1.50 % · S 0.06 – 0.25 % · Fe Remainder
- Specifications
- DIN 8201; BS 2451
- Packaging
- 25 kg sacks on pallet up to 1 t; 1 ton loose in a big bag
- Blasting Systems
- Pressure blast system, Wheel blasting system
Available sizes
| Designation | Average grain size (mm) |
|---|---|
| R 34 | 0.8 – 1.25 |
| R 39 | 1.00 – 1.40 |
| R 47 | 1.20 – 1.70 |
| R 55 | 1.40 – 2.00 |
| R 66 | 1.70 – 2.40 |
| R 80 | 2.00 – 2.80 |
| R 95 | 2.40 – 3.35 |
| R 111 | 2.80 – 4.00 |
| R 132 | 3.35 – 4.75 |
| W 1 | 0.00 – 8.00 |
| W 2 | 4.00 – 8.00 |
| W 3 | 4.50 – 6.00 |
| W 4 | 5.00 – 8.00 |
| R 0.5 | 0.5 – 0.80 |
| R 0.8 | 0.80 – 1.25 |
| R 1.0 | 1.00 – 1.40 |
| R 1.4 | 1.40 – 2.00 |
| R 1.8 | 1.80 – 2.60 |
| R 2.2 | 2.2 – 3.00 |
| R 2.8 | 2.8 – 3.40 |
| R 3.2 | 3.20 – 4.30 |
| R 3.6 | 3.60 – 5.30 |
| R 5.0 | 5.00 – 7.80 |
| R 6.0 | 6.00 – 9.80 |
Blasting applications
- Heavy concrete
- Pyrotechnics
- Radiation protection
- Weighting material
Advantages
- Reusable abrasive
Other grain sizes can be produced if required.