Blasting abrasives supplier
+90 216 706 70 72+90 532 063 81 58info@anadolukumlama.com

Mineral abrasives

Pink fused alumina

Pink fused alumina, tougher and longer-lasting thanks to chromium oxide.

Pink fused alumina, close-up view

Our customers use both pink fused alumina and white fused alumina as a blasting medium and abrasive. However, the addition of chromium oxide makes pink fused alumina tougher and more durable.

Technical specifications

Hardness
9 mohs
Grain shape
angular
Melting point
ca. 2.050 °C
Specific gravity
ca. 3.9 – 4.1 g/cm³
Bulk density (depending on grain size)
ca. 1.3 – 2.0 g/cm³
Typical Chemical Analysis
Al₂O₃ 99.30 % · Cr₂O₃ 0.30 % · Na₂O 0.30 % · Fe₂O₃ 0.05 % · CaO 0.05 %
Specifications
FEPA F; FEPA P; EN ISO 11126-7; DIN ISO 8486-1; MIL A-A-59316; ANSI B74-12; JIS R6001; D50TF5 Class A+D
Approvals
CSS12 (Rolls-Royce)
Packaging
25 kg bags on 1t pallets; 1 ton loose in a big bag
Blasting Systems
Pressure blast machines, Vacuum blast machines

Available sizes

FEPAAverage grain size (µm)
F 0082000 – 2800
F 0101700 – 2360
F 0121400 – 2000
F 0141180 – 1700
F 0161000 – 1400
F 020850 – 1180
F 022710 – 1000
F 024600 – 850
F 030500 – 710
F 036425 – 600
F 040355 – 500
F 046300 – 425
F 054250 – 355
F 060212 – 300
F 070180 – 250
F 080150 – 212
F 090125 – 180
F 100106 – 150
F 12090 – 125
F 15063 – 106
F 18053 – 90
F 22045 – 75

Blasting applications

  • Bonded grinding wheels
  • Dry abrasive
  • Fine abrasive
  • Grinding media on underlay
  • Wet abrasive

Advantages

  • Reusable abrasive

Other grain sizes can be produced if required.

Which material and grain size suit your job?

Tell us about your surface, your blasting system and the quantity you need, and our sales team will get back to you.