Cast stainless steel round Cr shot is an attractively priced alternative to cast stainless steel round CrNi for the machining of aluminium castings and other non-ferrous materials. In the operating mixture, this chromium blasting agent reaches a high hardness, which allows fast working.
Technical specifications
- Product code
- Cr
- Hardness of the new grain
- +/- 40 HRC (390 HV)
- Hardness in operating mixture
- +/- 50 HRC (530 HV)
- Grain shape
- irregular
- Melting point
- ca. 1.450 – 1.500 °C
- Specific gravity
- ca. 7 g/cm³
- Bulk density (depending on grain size)
- ca. 3.8 – 4.6 g/cm³
- Microstructure
- martensitic
- Typical Chemical Analysis
- Cr 12.00 – 20.00 % · Si max. 4.00 % · Mn max. 2.00 % · Ni max. 0.95 % · C max. 0.30 %
- Packaging
- 25 kg bags on 1t pallets; 1 ton loose in a big bag
- Blasting Systems
- Pressure blast machines, Wheel blast machines
Available sizes
| Designation | Average grain size (mm) |
|---|---|
| BETA 010 | 0.0 – 0.2 |
| BETA 020 | 0.1 – 0.3 |
| BETA 030 | 0.2 – 0.5 |
| BETA 040 | 0.4 – 0.8 |
| BETA 050 | 0.6 – 1.0 |
| BETA 060 | 0.7 – 1.2 |
| BETA 100 | 1.0 – 1.4 |
| BETA 150 | 1.2 – 1.7 |
| BETA 200 | 1.4 – 2.0 |
| BETA 300 | 1.7 – 3.2 |
Blasting applications
- Deburring
- Descaling
- Micro blasting
- Sand removal
- Structural blasting
- Surface finish
- Sweep blasting of zinc-plated parts
Advantages
- Reusable abrasive
Other grain sizes can be produced if required.