The inner layer of Contracor ExtraBlast blast hoses is abrasion-resistant, black, conductive natural rubber (NR). Reinforcement is made of high-strength textile cords, and the cover is an abrasion- and ozone-resistant, pin-pricked, black conductive SBR/NR blend. Abrasion loss according to DIN 53516 is at most 60 mm³, with an average of 52 mm³. The operating temperature is between –30 °C and +80 °C, the safety factor is 3:1, and tolerances comply with RMA class 311-A.

| Model | Inner x outer diameter | Roll length |
|---|---|---|
| Contracor ExtraBlast-13 | 13 x 27 mm | 5 m, 20 m, 40 m |
| Contracor ExtraBlast-19 | 19 x 33 mm | 20 m, 40 m |
| Contracor ExtraBlast-25 | 25 x 39 mm | 20 m, 40 m |
| Contracor ExtraBlast-32 | 32 x 48 mm | 20 m, 40 m |
The Twinline hose for remote control has a diameter of 6 mm and is supplied with fittings attached in 5 m, 20 m and 40 m rolls.
Nylon NHP nozzle holders fit Contracor nozzles with their 50 mm thread and come with a rubber gasket and screws. Blast hose quick couplings are available in nylon (CQP) or in zinc-plated, yellow-passivated malleable iron (CQT); they are compatible with the CFT hose couplings on Contracor blasting machines and are supplied with a rubber gasket, screws and a safety clip. Spare rubber gaskets are also available separately for each size.

| Hose size | Nozzle holder (nylon) | Coupling (nylon) | Coupling (metal) |
|---|---|---|---|
| 13 x 27 mm | NHP-0 | CQP-0 | CQT-0 |
| 19 x 33 mm | NHP-3/4 | CQP-3/4 | – |
| 25 x 39 mm | NHP-1 | CQP-1 | CQT-1 |
| 32 x 48 mm | NHP-2 | CQP-2 | CQT-2 |