Well Gravel and Drainage Gravel: What They Are and What to Look For

The role and selection of well (filter) gravel used in water wells and drainage gravel used in foundation and garden drainage, and the properties of quartz gravel.

Published: · 5 min read

Round-grained quartz gravel used in well drilling and drainage work

Well gravel (gravel pack) and drainage gravel are both used to let water pass while holding back soil and fine particles. One works in a water well, the other in foundation, retaining wall and garden drainage. In this article we explain the role of each gravel, what it should be like, what size is chosen and why quartz gravel is preferred.

What is well gravel (filter gravel)?

After a water well is drilled, a screened (slotted) pipe is lowered into it. The screened gravel filled into the annular space between the outside of the pipe and the borehole wall is called well gravel, filter gravel, gravel pack or gravel envelope.

This gravel has two jobs: to prevent fine sand and silt in the water-bearing layer (aquifer) from entering the well, and to let water flow freely into the pipe. Gravel that is not chosen correctly can lead to sand in the well, pump wear or a drop in well yield. For the concept of an aquifer, see the aquifer article on Wikipedia.

What should well gravel be like?

  • Round-grained: Regular, permeable voids form between round grains; the gravel settles easily around the pipe and moves down without bridging.
  • Clean: It should be free of clay, dust and organic matter, and washed if necessary.
  • High silica content: Soluble grains such as limestone can dissolve during the acid cleaning treatments used in well maintenance. Quartz gravel with a high silica content is more durable in this respect.
  • Narrow and correct grain range: The gravel size is chosen according to the grain size distribution of the sand in the aquifer and the slot opening of the screen pipe.

What size should well gravel be?

There is no single correct size. On the market, well gravel is referred to by grain ranges such as 7 – 15 mm, but the correct range is determined separately for each well. Gravel that is too coarse cannot hold back fine sand; gravel that is too fine can pass through the screen slots or slow down the water flow.

This selection is made by the drilling company or a hydrogeologist, based on the soil samples taken during drilling. When ordering gravel from a supplier, it is enough to give the grain range in the project. Our well gravel is in the 5 – 15 mm range.

Screened quartz sand grains used in filter layers
Finer filter layers use screened quartz sand of the same mineral.

What is drainage gravel and where is it used?

Drainage gravel is a coarse gravel used to collect excess water in the ground and direct it to a drainage pipe or away from the site. Common uses include:

  • Around building foundations and basement retaining walls
  • Behind retaining walls
  • Around and above perforated drainage pipes
  • Garden, landscape and sports field drainage
  • Drainage trenches in road and infrastructure works

Drainage gravel is usually wrapped in geotextile fabric. The fabric prevents the surrounding soil from filling the voids in the gravel over time. The size of the drainage gravel and the type of fabric are specified in the project details. Our drainage gravel is in the 15 – 32 mm range.

Quartz gravel or crushed stone?

Both natural round gravel and crushed stone can be used in drainage. The differences are:

  • Round gravel: The voids between grains are regular, water passes easily and it is easy to place. Round grains are preferred for well gravel.
  • Crushed stone: Angular grains interlock and shift less in load-bearing fills. However, the dust from crushing can reduce permeability if it is not washed.

Which one the project calls for depends on the ground and load conditions.

Technical values of our quartz gravel

Quartz gravel is a natural, round-grained gravel made up largely of silicon dioxide (SiO₂). The values from accredited laboratory (TS EN ISO 17025) analyses are as follows:

ProductGrain range (mm)SiO₂ (%)Al₂O₃ (%)Fe₂O₃ (%)
Well gravel5 – 1596.911.500.345
Drainage gravel15 – 3299.010.400.132

The values belong to the sample and may vary from batch to batch. The hardness of quartz is 7 Mohs. We deliver the gravel in 25 – 50 kg bags, 1.5 tonne big bags or in bulk by truck.

Bagged products stocked on pallets in the warehouse
Bagged and big bag products are stocked on pallets in our warehouse.

Frequently asked questions

What size should well gravel be?

The correct range is determined by the drilling company or a hydrogeologist according to the grain size distribution of the sand in the aquifer and the slot opening of the screen pipe. If you send us the range in your project, we will assess the suitable product or the option of custom screening together.

Can crushed stone be used instead of drainage gravel?

Crushed stone can also be used in many drainage jobs. What matters is that the material is clean and coarse enough and matches the grain range in the project details. Dusty material reduces permeability.

Is quartz gravel used in water treatment?

Yes. Quartz gravel is also used as the bottom support layer of the filter bed in the sand filters of water treatment plants. We explained the use of filter sand in our pool filter sand article.

Request a quote for well and drainage gravel

Specify the grain range, quantity, delivery method and delivery location you need in the quote form. We also supply construction sand for concrete and mortar work and quartz sand for filter and fill work. We compared sand types in our types of construction sand article.