Quartz Sand for Epoxy Floors: Broadcast and Filler Sand

How quartz sand is used as broadcast and filler sand in epoxy floor coatings, why the sand must be dry and dust-free, and how to choose the grit size.

Published: · 5 min read

Dry quartz sand used as broadcast and filler sand in epoxy floor coatings

Most epoxy coatings used on factory, warehouse, car park and workshop floors also contain quartz sand. The sand gives the coating slip resistance, abrasion resistance and build thickness. This is the product people search for as "quartz sand for epoxy floors", "epoxy flooring sand" or "silica sand for epoxy". In this article we explain where quartz sand is used in epoxy floors, why it must be dry and screened, and how the grit size is chosen.

What does quartz sand do in an epoxy floor?

  • Slip resistance: In wet or oily areas, sand broadcast onto the surface creates a rough, anti-slip texture.
  • Abrasion and impact resistance: The hardness of quartz (7 Mohs) helps the coating wear more slowly under traffic.
  • Build and filling: In self-levelling and mortar-type systems, the sand is mixed with the resin to form a thicker and more economical layer.
  • Intercoat adhesion: Sand broadcast onto the primer leaves a rough surface that the next coat can key into mechanically.

For general information about epoxy resin itself, see the Wikipedia article on epoxy.

Broadcast sand vs filler sand

Quartz sand enters epoxy systems in two ways:

  • Broadcast (seeding) sand: It is scattered over the primer or intermediate coat by hand or by machine while the coat is still wet. Once the coat has cured, the loose excess sand is swept off and the top coat is applied. Anti-slip floors and thick coatings are built this way.
  • Filler (mix-in) sand: It is mixed with the resin in a set ratio. Fine fractions are used in self-levelling coatings and coarser fractions in mortar-type (trowel-applied) coatings.

The mixing ratio, the broadcast rate and the order of coats are given in the technical data sheet of the epoxy system used. Because these values vary from manufacturer to manufacturer, the data sheet should be followed.

Bagged and big bag products shipped with the company vehicle
Quartz sand orders also go out with our own vehicles, and we ship across Türkiye by cargo.

Why must the sand be dry and dust-free?

Epoxy resin is sensitive to moisture and dust. The condition of the sand directly affects the result of the coating:

  • Moisture: Damp sand can affect the curing of the resin and lead to blistering, whitening and adhesion problems. That is why kiln-dried or dried sand is used in epoxy work.
  • Dust and clay: Fine dust on the surface of the grains weakens the bond between the resin and the sand and increases the amount of resin needed in a filler mix.
  • Narrow grain range: Screened sand leaves an even texture on the surface, while sand with a wide grain range gives an irregular appearance.

The quartz sand we supply is screened without crushing and dried with hot air at a maximum of 120 °C.

Which grit size should you choose?

The fraction is chosen according to the type of system and the desired texture. As a general guide:

Fraction (mm)Typical use in epoxy floors
0.1 – 0.5Filler in self-levelling coatings, fine texture
0.5 – 1.0Broadcast onto primer and intermediate coat, medium slip resistance
0.8 – 1.5More pronounced slip resistance, mortar-type coatings
1.5 – 2.5 and aboveThick mortar-type and heavy-duty floors

This table is a starting point. The exact fraction is determined by the epoxy system manufacturer's technical data sheet and the service conditions of the floor. If the data sheet calls for a different grain range, custom screening can be done.

Quartz sand or silica sand?

In epoxy work, "silica sand" and "quartz sand" usually refer to the same material: sand consisting largely of silicon dioxide (SiO₂). The SiO₂ content of our quartz sand is 89.6 – 91.5% depending on the fraction. We explain the difference between the terms in our article quartz sand vs silica sand.

Safety during application

Dust is generated when quartz sand is broadcast and swept. This dust may contain respirable crystalline silica. A suitable dust mask should be worn while broadcasting sand and sweeping off the excess, enclosed areas should be ventilated and the dust should be collected by vacuum where possible. For the risks of silica dust, see our article silica dust and occupational safety. For the safety precautions for epoxy resin and hardener, follow the products' safety data sheets (SDS).

Bagged quartz sand stocked on pallets in the warehouse
Quartz sand is delivered from stock in 25 – 50 kg kraft bags and 1.5 tonne big bags.

Frequently Asked Questions

Can construction sand be mixed into epoxy?

It is not recommended. Construction sand is usually not dried, has a wide grain range and may contain fine materials such as dust and clay. These adversely affect the adhesion and curing of the resin. Dried and screened quartz sand should be used.

How much broadcast sand is needed per square metre?

The amount depends on the thickness of the coat, the fraction of the sand and whether the sand is broadcast to refusal. The technical data sheet of the epoxy system you use gives the recommended amount per square metre.

Do you supply coloured quartz sand?

The quartz sand we supply has a natural yellowish-beige colour. Decorative coloured coatings use specially dyed sands; you can state your requirement in the quote form.

Request a quote for epoxy sand

State the system you use, the required fraction and the quantity in the quote form, and we will choose the right quartz sand together. For other uses of quartz sand, see our article uses of quartz sand, and for other types of sand, our article types of construction sand.