Construction sand is not a single product. On the same site, the sand that goes into concrete and the sand used in the final coat of plaster are not the same; grain size, cleanliness and grain shape change with the job. In this article we cover the construction sand types, the differences between coarse sand, plastering sand, finishing sand and concrete sand, where river sand and crushed sand fit, and how to tell good sand.
What is construction sand?
Construction sand is the fine aggregate used in concrete, mortar, plaster and fill work. Aggregate is the granular material that, together with cement and water, forms the skeleton of concrete or mortar. Sand is the fine part of this skeleton and fills the voids between the coarse aggregate grains of gravel or crushed stone.
In Türkiye, the TS 706 EN 12620 standard is the basis for concrete aggregates and TS EN 13139 for mortar aggregates. These standards and the project specification determine which grading and which cleanliness limits are required. For a general definition of sand, see the Wikipedia article on sand.
Sand types by source
The first thing that distinguishes sand is where it comes from. This directly affects the shape of the grains and the contaminants they contain.
- River sand: Natural sand taken from riverbeds. Because water wears the grains down, they are round and smooth. It is easy to work, but it may contain clay and organic matter, so it needs to be washed and screened.
- Pit sand: Natural sand extracted from sand and gravel pits. It is screened and, where necessary, washed to separate it into different grain ranges.
- Crushed sand: Produced by crushing rocks such as limestone and basalt in crushing plants. Its grains are angular and interlock well in concrete; however, its dust content can be high and it is harder to work than natural sand.
- Sea sand: Contains salt (chloride). Because chloride can cause reinforcement corrosion in reinforced concrete, sea sand should not be used in a structure without being washed and checked.

By use: coarse sand, plastering sand and finishing sand
On site, sand is mostly named after where it will be used:
- Coarse sand: Covers a wide grain range from fine to coarse grains. It is used in concrete, masonry mortar, screed and infrastructure fill. The coarse sand we supply is in the 0 – 5 mm range.
- Plastering sand: Sand with the coarse grains screened out, for the base coat of plaster. The sieve opening varies with the plasterer's preference and the type of plaster; coarse grains cause roughness and a risk of cracking in the plaster.
- Finishing sand: Fine-grained, clean sand used in the final coat of plaster (the finish coat). For an even, smooth surface it is important that it is fine and uniform.
- Screed and fill sand: Used for jobs such as floor screed and pipe bedding; again, cleanliness and grading are chosen according to the job specification.
| Our product | Grain range | Main use |
|---|---|---|
| Coarse sand | 0 – 5 mm | Concrete, mortar, infrastructure fill |
| Finishing sand | Fine-grained | Plaster finish coat, fine mortar |
Full product information is on our construction sand page.
What should concrete sand be like?
In concrete, the role of sand is to bring the coarse aggregate and the cement paste together to give a void-free, workable mix. Good concrete sand should have the following properties:
- Cleanliness: Clay, silt and organic matter should be low. These fine materials prevent the cement from coating the grains and reduce strength.
- Continuous grading: Fine, medium and coarse grains should be balanced; single-sized sand requires more cement paste.
- Sound grains: Grains that crumble easily or are soft or flaky are not wanted.
- Freedom from salt: Chloride content is limited in reinforced concrete, so unwashed sea sand is not used.
Ready-mix concrete plants check the suitability of sand with laboratory tests. If you are mixing concrete yourself on site, ask your supplier for an analysis of grading and fines content.
How to tell good sand on site
These checks do not replace a laboratory test, but a few simple checks help weed out bad sand from the start:
- Hand check: Squeeze damp sand in your hand and let it go. If a mud-like layer stays on your hand, the clay and silt content may be high.
- Jar (settling) test: Put some sand and water in a clear jar, shake it and let it stand. If a thick layer of mud builds up on top of the sand, the sand is dirty.
- Visual check: There should be no foreign matter such as roots, leaves or bits of coal, and no excessively large grains.
- Smell and colour: A smell of rotting plants or a very dark colour can be a sign of organic matter.
Packaging and delivery
We deliver construction sand in three ways, depending on the size of the job: 25 – 50 kg bags, 1.5 tonne big bags and bulk by truck. Bags and big bags make it easier to store the material on site without it spreading or getting wet; for large quantities, bulk delivery is more practical.

For jobs such as water treatment, filters and floor coatings we also supply dried quartz sand with narrower grain ranges, and quartz gravel for drainage and drilling work. We explain how gravel is used in our article on drilling and drainage gravel.
Frequently asked questions
Are plastering sand and concrete sand the same?
No. Concrete sand can have a wide grain range, while plastering sand is a finer sand with the coarse grains screened out. The sand used for the finish coat is finer still. The wrong sand can cause cracks and roughness in plaster and loss of strength in concrete.
Can sea sand be used in construction?
Because sea sand contains salt (chloride), it should not be used in a structure, especially in reinforced concrete, without being washed and having its chloride content checked. Chloride can cause the reinforcement to rust.
Can construction sand be used for sandblasting?
We do not recommend it. Construction sand can contain a high proportion of free crystalline silica; in blasting it breaks down quickly and creates heavy dust. Abrasives such as garnet or aluminium oxide should be used for blasting. Details are in our article on safety in sandblasting.
Request a quote for construction sand
Tell us in the quote form the type of sand you need, the approximate quantity, the delivery method (bag, big bag or bulk) and the delivery location, and we will get back to you with a suitable quote. You can browse our other products on our products page.