The heart of the system that keeps pool water clear is the sand filter, and the performance of this filter depends largely on the sand inside it. The wrong sand or the wrong layer order leads to cloudy water and a filter that clogs often. In this article we explain what pool filter sand should be like, the order of the layers, and when and how to replace the sand.
How does a sand filter work?
The pump pushes pool water into the filter tank. The water enters at the top of the tank, trickles down through the sand bed and returns to the pool through the collector pipes (laterals) at the bottom of the tank. The narrow gaps between the sand grains trap dirt and suspended particles in the water.
Over time the sand bed fills with dirt and the filter pressure rises. At that point a backwash is carried out: water is sent in the reverse direction, the sand bed lifts and the accumulated dirt is flushed out through the waste line. For the general principle of the method, see the Wikipedia article on the rapid sand filter.
What should pool filter sand be like?
- It should be quartz (silica) sand: Because it is hard and chemically resistant, it does not dissolve with pool chemicals and does not wear down during backwashing.
- It should be screened to a narrow grain range: The filter's retention capacity and its behaviour during backwashing depend on grain size. The grain range should match the filter manufacturer's recommendation.
- It should be clean and dust-free: Dust and clay pass into the pool at the first start-up and clog the filter.
- Construction sand should not be used: Because of its wide grain range and fines content, it clogs the filter quickly and makes the water cloudy.
How many kilograms of sand your filter takes and which grain range it requires are usually stated on the tank label or in the user manual. Use this information as the basis when buying sand.
Pool filter sand layer order
In most filters the sand is not filled as a single layer but in layers that become finer from bottom to top:
- Bottom layer, support gravel: It covers the collector pipes (laterals), prevents sand from escaping through these pipes and ensures the water is distributed evenly across the base.
- Middle layer, coarse sand: In some filters it is used as a transition layer between the gravel and the fine sand.
- Top layer, filter sand: The finer, narrow-range sand that does the actual filtering.
The number of layers and the grain range and height of each layer vary by filter model. In small domestic filters a single layer of sand may be sufficient. Following the manufacturer's diagram is the safest way.

When should pool filter sand be replaced?
The service life of the sand varies with how heavily the pool is used, the water chemistry and the maintenance routine; it would not be right to give a fixed period. The following signs may indicate that it is time to replace the sand:
- Filter pressure rising again shortly after a backwash
- Water not clear even though the chemical values are correct
- Sand clumping or hardening; water channelling through the sand and passing without being filtered
- Sand appearing during backwashing or on the pool floor (this can also be a fault in the collector pipes)
How is pool filter sand replaced?
The general steps are below; for details, follow the filter manufacturer's manual, and cut the power to the pump before starting work.
- Stop the pump, close the valves and drain the water from the tank.
- Remove the lid or the multiport valve and take out the old sand with a scoop or a wet vacuum.
- Check the collector pipes (laterals) for breaks or cracks and replace them if necessary.
- Fill the tank halfway with water to protect the laterals.
- First add the support gravel, then slowly fill the sand up to the level specified by the manufacturer.
- Refit the lid and run a few minutes of backwash followed by a rinse to flush the dust out of the new sand.
Our quartz sand fractions
We supply quartz sand screened without crushing and dried with hot air at no more than 120 °C, in six fractions between 0.1 and 5 mm: 0.1 – 0.5 · 0.5 – 1.0 · 0.8 – 1.5 · 1.5 – 2.5 · 2.0 – 3.0 · 3.0 – 5.0 mm. The SiO₂ content of the fractions is approximately 90%. If your filter requires a different grain range, custom screening can be done as needed. We also supply quartz gravel for the bottom support layer.

Frequently Asked Questions
Can construction sand be put in a pool filter?
It is not recommended. Construction sand has a wide grain range and may contain fine materials such as clay and dust. These materials quickly clog the filter and make the pool water cloudy. Screened, clean quartz sand should be used.
How many kg of sand does a pool filter need?
The amount varies with the diameter and model of the filter tank. The correct amount is usually stated on the tank label or in the user manual.
Are quartz sand and silica sand the same thing?
In everyday use they mostly describe the same material: sand made up largely of silicon dioxide. We explain the difference in our article the difference between quartz sand and silica sand.
Request a quote for filter sand
State the grain range and quantity your filter requires in the quote form, and let's choose the right fraction together. For other uses of quartz sand, see our article quartz sand applications, and for gravel, our article drilling and drainage gravel.