Blasting abrasives supplier
+90 216 706 70 72+90 532 063 81 58info@anadolukumlama.com

Workplace Safety

Blasting Waste: Waste Code, Hazards and Disposal

The waste code of spent abrasive and blasting dust, how hazardous status is decided, the hazards of blasting dust and ways to reduce blasting waste.

Published: · 5 min read

Steel shot abrasive that can be reused many times through recovery

At the end of a blasting job you are left with spent abrasive, removed paint and rust, mill scale and dust. This mixture is often treated like ordinary rubble, but from a regulatory point of view it is waste that must be recorded and disposed of correctly. In this article we explain the waste code of blasting waste in Turkey, how it is decided whether it is hazardous, the hazards of blasting dust and the ways to reduce the amount of waste.

What does blasting waste contain?

  • Spent abrasive: Broken and pulverised abrasive grains.
  • Removed coating: Old paint, primer, antifouling paint or other coatings.
  • Rust and mill scale: Iron oxides removed from the steel surface.
  • Other contaminants: Oil, salt and other substances from the treated surface.

Whether the waste is hazardous is usually determined not by the abrasive itself but by the material removed from the surface. For example, the waste from a job where old paint containing lead or chromate is removed is very different from the waste produced by descaling a new steel sheet.

The waste code of blasting waste

In Turkey, waste is classified according to the list of wastes annexed to Turkey's 2015 Waste Management Regulation (Atık Yönetimi Yönetmeliği). This list contains two codes for blasting waste:

Waste codeDescriptionWhen
12 01 16*Waste blasting material containing hazardous substancesIf the removed coating or the surface contains hazardous substances
12 01 17Waste blasting material other than those mentioned in 12 01 16Waste found not to contain hazardous substances

The asterisk (*) marks hazardous waste. These two codes are "mirror" codes of each other: which one applies is decided by looking at the content of the waste. The decision is mostly based on a laboratory analysis of the waste. As the regulation and the list of wastes may be updated over time, check the current legislation and the guidance of the provincial environment directorate before applying them. These codes come from the European List of Waste, and local rules differ in other countries. For general information, see the Wikipedia article on waste management.

The hazards of blasting dust

  • Respiratory tract: Blasting dust contains fine respirable particles. In blasting with silica-containing sand, crystalline silica dust can cause serious lung diseases.
  • Heavy metals: Substances from old paints such as lead, chromium or copper can be inhaled with the dust or mix into soil and water.
  • Environment: Uncontrolled dust spreads with the wind and is carried into drains by rain.

Workers should use a blasting helmet, suitable respiratory protection and a dust collection system. Details are in our article on blasting safety and silica dust. In case of persistent respiratory complaints, the workplace physician should be consulted.

Garnet abrasive used with low dust in open-air blasting
Abrasives that break less produce less dust and less waste.

How is blasting waste stored and disposed of?

  • Collect it separately: Do not mix blasting waste with other waste; keep hazardous and non-hazardous waste apart.
  • Store it closed and labelled: Keep the waste in big bags or closed containers, in an area protected from rain and wind, with a label showing the waste code.
  • Hand it to a licensed company: The waste is delivered to a transport and disposal/recovery company holding an environmental licence. Hazardous waste shipments are recorded through MoTAT (Mobil Atık Takip Sistemi), Turkey's mobile waste tracking system.
  • Keep records: The quantity of waste and the delivery details are reported in the waste declaration made through the Ministry's online systems.

The details of the obligations vary with the type of business and the amount of waste. Get support on this from your environmental consultant or the provincial environment directorate.

Ways to reduce blasting waste

The cheapest waste is the waste that is never produced. The choice of abrasive directly affects the amount of waste:

  • Use a recyclable abrasive: Steel shot and steel grit are used many times in cabinets with recovery and in wheel blast machines; the abrasive waste generated for the same job drops sharply.
  • Choose an abrasive that breaks less: Cheap single-use sands quickly turn into dust. Tough abrasives such as garnet produce less dust and can be used several times in suitable systems.
  • Keep the recovery system well maintained: The dust separator and screen separate usable grains from dust and return the abrasive to the system. Details are in our article on abrasive recovery.
  • Choose the right grit size: An abrasive coarser than necessary consumes more abrasive. For selection, see our article on grit size selection.
Steel grit used in blasting systems with recovery
Steel grit reduces abrasive waste by being used many times in systems with recovery.

Frequently asked questions

Is blasting dust hazardous waste?

Not always. The list of wastes has two codes: 12 01 16* (hazardous) and 12 01 17 (non-hazardous). Which one applies is decided according to the content, especially of the removed coating, with an analysis if necessary.

Can spent blasting sand be used as fill or in construction?

Spent abrasive is waste; without a recovery permit in line with the legislation it cannot be used as fill, in roads or in construction. Recovery can only be carried out through licensed facilities.

Does steel shot waste also count as blasting waste?

Spent metallic abrasive and dust from the blasting process are also blasting waste and are classified in the same way. The advantage of metallic abrasives is that, because they are used many times, the total amount of waste is small.

The right abrasive for less waste

Describe your blasting system and the work you do in the quote form, and let us choose together the abrasive that will reduce waste and consumption. You can browse all products on our products page.

Which material and grain size suit your job?