Blasting abrasives supplier
+90 216 706 70 72+90 532 063 81 58info@anadolukumlama.com

Technical Information

What Is Mill Scale? How It Forms and How to Remove It

How mill scale forms on hot-rolled steel, why it damages paint, and the methods used to remove it, with abrasive blasting first among them.

Published: · 6 min read

Angular steel grit abrasive used for mill scale removal

The dark grey, slightly shiny layer on a newly bought steel sheet or section is often mistaken for rust. This layer is mill scale. It forms as part of steel production, and although at first glance it seems to protect the surface, it is a serious risk for paint and coatings. In this article we explain what mill scale is, how the mill scale layer forms, why it should not be left under paint and which methods are used to remove it.

What is mill scale?

Mill scale is the iron oxide layer that forms on the surface of steel when it comes into contact with air at high temperature. During processes such as hot rolling, forging and heat treatment the steel surface oxidises, and as it cools this oxide turns into a thin crust that adheres tightly to the surface.

Mill scale is not a single substance but several overlapping iron oxide layers: wüstite (FeO) lies closest to the steel, magnetite (Fe₃O₄) is in the middle, and a thin layer of hematite (Fe₂O₃) is on the outside. For general information, see the mill scale article on Wikipedia.

How does the mill scale layer form?

  • Hot rolling: Mill scale forms on the surface while sheets, plates and sections are rolled at high temperature. This is why almost all hot-rolled steel carries mill scale.
  • Forging and heat treatment: Forged parts heated in a furnace and parts that undergo heat treatment also build up mill scale.
  • Welding: The heat creates a thin oxide layer on and around the weld seam.

Cold-rolled sheets, on the other hand, have no mill scale or very little of it; surface preparation on these sheets is a different matter.

Why should mill scale not be left under paint?

At first glance mill scale looks sound and protective, but it causes two major problems for paint:

  • It cracks and flakes off over time: Mill scale and steel expand at different rates. With temperature changes and vibration, the mill scale cracks, flakes off and takes the paint on top of it along with it.
  • It accelerates corrosion: Mill scale is electrochemically more noble than steel. Where the mill scale cracks, the exposed steel behaves like a battery with the mill scale, and rust progresses faster at these points.

For this reason, paint and coating specifications, especially for harsh environments, require mill scale to be removed completely. The Sa 2½ cleanliness grade describes a surface from which mill scale, rust and old coatings have been visibly removed. We explain the grades in our article on Sa 2, Sa 2½ and Sa 3.

Mill scale removal methods

  • Abrasive blasting: An angular abrasive breaks up and strips the mill scale and at the same time creates the profile that the paint will grip. It is the most common and most reliable method for removing mill scale.
  • Acid pickling: Parts are freed of mill scale in an acid bath. It is used before galvanising and in series production such as wire and pipe; it requires acid waste handling and neutralisation, and it does not create a surface profile.
  • Wire brushing and grinding: These remove loose mill scale but cannot fully strip tightly adhering mill scale, and they can polish the surface. They are not sufficient except for small repairs.
  • Weathering: Leaving steel outdoors and waiting for the mill scale to come off with rust is an old method. It is slow, rusts the surface unevenly, and blasting is still needed in the end.
Brown aluminium oxide used for blasting steel surfaces covered with mill scale
With its hard, angular grains, brown aluminium oxide strips mill scale quickly.

Which abrasive is used for mill scale removal?

Because mill scale is a hard, tightly adhering layer, angular and hard abrasives are preferred. The choice depends on where the work is done and whether the system recovers the abrasive:

  • Steel grit: Used many times over with recovery in blast cabinets and wheel blasting machines. It is the main abrasive for mill scale removal on sheet and section lines.
  • Brown aluminium oxide: With its hard, sharp grains it strips quickly in cabinet and pressure blasting.
  • Garnet: Used in pressure blasting outdoors and on site, with low dust and an even surface.
  • Stainless cut wire: The product data lists descaling and casting cleaning among its uses; it can be considered for work where iron contamination is unwanted.

On wheel blasting lines, steel shot and steel grit are usually mixed in a set ratio so that mill scale removal and the required profile are achieved together. For details, see our article on the difference between steel shot and steel grit.

Stainless steel cut wire used for casting cleaning and mill scale removal
With its long-lasting grains, stainless cut wire is used for mill scale removal and casting cleaning in wheel blasting machines.

Points to watch in mill scale removal

  • Check the result visually: Areas where mill scale remains look dark and slightly shiny. Edges, corners and the areas around welds are the places most often missed.
  • Do not delay painting: Cleaned steel can rust again quickly in humid air.
  • Renew the abrasive: Broken and dusty grains in recovered abrasive reduce cleaning speed; the screen and dust separator need to work properly at all times.
  • Do not use sand containing silica: The dust generated during blasting is a risk to the respiratory tract. Details are in our article on occupational safety in blasting.

Frequently asked questions

Is mill scale rust?

No. Mill scale is an iron oxide layer that forms while steel is at high temperature; rust is the corrosion product that forms on steel over time through moisture and oxygen. Rust does, however, start faster where mill scale has cracked.

Can you paint over mill scale?

It is not recommended. Mill scale cracks and flakes off over time and takes the paint on top of it with it. For a lasting paint and coating, mill scale must be removed by blasting; the required cleanliness grade is set by the paint specification.

What is mill scale dust used for?

Mill scale collected from rolling and forging operations is used as a raw material in some industrial processes because of its iron oxide content. In blasting, however, mill scale is waste; it is collected together with the blasting dust and disposed of in accordance with waste regulations.

Request a quote for mill scale removal abrasives

Tell us about the parts you will clean, the blasting system you use and the required cleanliness grade in the quote form, and let us choose the right abrasive and grit size together. You can browse all products on our products page.

Which material and grain size suit your job?

Tell us about your surface, your blasting system and the quantity you need, and our sales team will get back to you.